Skip to main content

HIAD Causes: Job Factors


This event occurred at the hydrogen 70 MPa dispenser of a refuelling station during the testing phase. Just after the start of the refuelling test, at a pressure of approximately 13 MPa, the…

An explosion occurred on a ship loaded with a cargo of 2333 tonnes of unprocessed incinerator bottom ash. Flammable gas generated by the ash produced two explosions: the first one was in the…

At a water sports center, a 35-liter container of caustic soda (NaOH) spilled down an aluminum metal staircase leading to a technical room housing other chemicals and electrical cabinets. Hydrogen…

A release of hydrogen and steam occurred in the battery room of a nuclear power plant around 21 h. Site agents neutralised the batteries. Noting the failure of the smoke extractor, public…

The event occurred at the factory producing multilayer circuit boards by a multistep dip operation. An employee inadvertently mixed 55 gal of 50 percent hydrogen peroxide into 110 gal of 30 percent…
An explosion occurred in a electrolyser cell, blowing off the cell's vent cover and severing a low-pressure chlorine gas pipeline. , what caused a release of chlorine in the building, The event…
A tube trailer-tractor transporting compressed hydrogen was travelling on a highway, when the driver lost the control of the vehicle trying to avoid an obstacle on the road. The vehicle collided with…

A trailer was transporting 35 tubes of compressed hydrogen (7 m3), when five of them fell, breaking the valves and releasing gas, which ignited on three of them. The caps designed to prevent the…

[Note of HIAD Validator: this is a preliminary event description, he CSB investigation is still ongoing] An explosion occurred on an isolation valve on the piping providing coke oven gas to a coke…

Early in the morning a hydrogen tube trailer experienced a tire fire and pulled onto the road shoulder. The driver attempted to extinguish the fire with the fire extinguisher on the vehicle. Heat…

A tube trailer was driving on a highway, when the drivers noticed in the back camera smoke coming from the rear of the vehicle. After stopping the vehicle on the shoulder, they discovered a fire…

This near miss occurred at metal smelting unit of a foundry. At 9:45 a. m. , due to a power outage, the cooling pumps of two furnaces containing nickel and chromium stopped. One of the two furnaces…

An empty fuel cells and hydrogen bus out of service was returning to the refuelling station, when it collided with a low bridge. This resulted in the rooftop hydrogen tanks being sheared off. The…

[Note HIAD validator: this an incident where a hydrogen system was affected, as effect of the initiating event, overpressure of LH2 tank with helium, but it is not a LH2 incident]. The second…

During the warm-up phase of a large liquid hydrogen sphere, the annular space was over-pressurised and perlite insulation was expelled through the evacuation nozzle and the burst diaphragm. Air…

A stainless steel manifold ruptured during experimental operation. The manifold was made of stainless steel and had a diameter of three inch (7. 5 cm). The hardware was off-the-shelf, slightly…

After a test of a LH2 vessel, during the warm up phase, the plan was to dispose of the hydrogen through the vent system. However, a leak to atmosphere occurred. This was due to a blind flange…

The incident affected the raw material buffer tank (design pressure 0. 38 MPa) of a diesel hydrogenation unit in a refinery. This buffer tank is located between the hydrogenation reactor and the raw…
The event occurred at one of the unit producing iron powder, consisting of a furnace with a running belt for the powder, kept under hydrogen atmosphere to reduce and purify the metal. The hydrogen…

The incident occurred at a chemical laboratory of a university. Six students were conducting experiments on producing nitrification carriers for waste leaching when an explosion followed by a fire…