A liquid hydrogen tanker (with a water capacity of 2000 l) was passing a highway interchange, when the safety valve of the tank activated, releasing hydrogen gas. The drivers stopped first on the…

A lightning strike ignited the hydrogen exiting a stack in a chemical factory. The hydrogen, produced by the chlorine electrolysis cells, was conveyed to the stack when the manufacturing unit using…
The leak occurred on a 44 m³ vehicle of liquid hydrogen during a delivery to the unloading station of a steel plant. The truck drivers had connected the tank container to the fixed storage managed by…
A 9000 gal (34 m3) LH2 storage tank exploded during repair of the vent stack. Few days before the explosion, the tank had been filled with LH2, but later on the hydrogen released and ignited at the…

A rupture disc opened on a 76 m3 (20,000-gallon) liquid hydrogen tank, causing the vent stack to release cold gaseous hydrogen. The gas ignited causing a fire on the vent stack's outlet.…

At a hydrogen production facility, the hydrogen compressor used to store hydrogen at approximately 20 MPa failed due to the rupture of the casing (spacer) connecting the hydraulic drive unit and…

This near-miss occurred at a company producing compressed gas bottles according to customers requests. When preparing a gas mixture containing oxygen and nitrogen, by mistake hydrogen was added,…

[NOTE of the EVENT VALIDATOR: this is a natural gas event, related to the NG supply chain. It may be however of interest for hydrogen-NG mixture transportation in pipeline. ] A 30-inch natural gas…

In 1987, well diggers had drilled a well for water, but had given up on one dry borehole at a depth of 108 meters. According to the source reported in the References, “…wind was coming out of the…
A potentially explosive situation was reported by safety inspectors at a nuclear waste tank. The waste slurry had formed a thick crust which was trapping hydrogen being continuously generated…
An operator noted a loose tube sheet flange stud on a high temperature, high pressure heat exchanger in an hydrodealkylation unit. The stud was found to be cracked through. Analysis proved to be made…
The incident occurred during a temporary shutdown of the distillate hydro-treatment unit. The crude oil distillation units main column overhead product was pumped to a gasoline storage tank via the…

The second stage of the Saturn V (S-II-T) was under full-duration static test, when one fire near LH2 valves of the LH2 tank and another in the engine area caused the automatic termination of the…

In a paper plant, an explosion occurs in a paper pulp tank while 2 workers were carrying out pipes cutting with a grinder on the roof of the tank. Detailed analysis of the event was performed by two…
The fire broke out on a worm ("vis sans fin") supplying a conveyor of aluminium. The ignition of the powder on the ground was caused by the flame cutting operation on the worm shell which generated…
The utility production facilities (electricity, water, air, and steam) at a refinery were isolated from the power grid and switched to two turbine generators in anticipation of a storm. However, at 9…
The vessel affected by the incident was a gas storage used for the hydro-desulphurisation process. The desulphurisation gas had high hydrogen content. The vessels had cracks in the upper transverse…
A hydrogen leak occurred at a tube bundle container at the loading and unloading bay of a PSA (Pressure Swing Adsorption) hydrogen production plant. During the hydrogen filling process, a worker in…
The bonnet of a 2-inch valve on a hydrogen quench line of a lube oil hydrotreater began to leak. 12 minutes later ignition occurred with fire engulfing the upper portion of the unit. The operative…
Release from a welding of a hydrogen transmission pipeline At 12:45 pm the operation control centre (OCC) recognised that a customer flow and pressure dropped significantly. At 13:28 the OCC made the…