Pressure vessel failure in a chemicals plant
The vessel affected by the incident was a gas storage used for the hydro-desulphurisation process. The desulphurisation gas had high hydrogen content. The vessels had cracks in the upper transverse fillet welds at the gas inlet which caused low stress brittle fractures. The cracks had been found during the maintenance, but not fixed. This eventually caused a gas release. Approximately 2. 5 hours after that a leak was detected and reported, a first explosion occurred. As the heat exchanger explosion was facing the desulphurisation pump room, the leaking gas gathered in the pump room, under the effect of the first explosion flame. 7 seconds later, a secondary explosion occurred in the desulphurisation pump room, resulting in 3 deaths. Due to the impact of debris from the first explosion and the high temperature of the open flame, a third explosion occurred in another cracked pressure pipe.
Event Date
June 28, 2015
Record Quality Indicator
Region / Country
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Causes
Cause Comments
the INITIATING CAUSE was corrosion of a welded joint, with a low brittle fracture resistance. One of the root CAUSES was a lack of maintenance and repair. Another could be attributed to lack of risk management and safety culture. The existence of the crack was known, but no action had been taken.