A fire in a first stage 'pygas' (pyrolysis of gasoline) hydrogenation of a naphtha cracker was caused by escape of a mixture of gasoline, hydrogen and nickel catalyst through a crack in…
A tube ruptured in the charge heater ('fired heater') of a desulphurisation reactor due to a blockage caused by accelerated coking. Flames spread over an area of some 100 feet outward…
This incident occurred a product purge vessel flange during planned maintenance activities on a chemical plant. The vessel had the function to collect unreacted gases from a polyethylene…
While a LH2 barge was being disconnected from dock, a flash occurred in the vent stack. No damage occurred but potential existed for major damage. [Ordin, NASA (1974)]