Skip to main content

Bourdon tube rupture due to hydrogen embrittlement (428)

This data is from the European Hydrogen Incidents and Accidents database HIAD 2.1, European Commission, Joint Research Centre.

Bourdon tube rupture due to hydrogen embrittlement

A Bourdon tube ruptured in pressure gauge after 528 hours of operation in LH2. The alarm sounded, the system was isolated and then vented. [Ordin, NASA (1974)]

Record Quality Indicator
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Cause Comments

The tube was made of martensitic stainless steel 403 SS which is subject to hydrogen embrittlement. It was requested that all gauges that have bourdon tubes be replaced with austenitic stainless steeel 303 SS.

Facility Information
Application Type
Application
LH2 vessel
Specific Application Supply Chain Stage
Components Involved

tube

Storage/Process Medium
Location Type
Location description

DESCRIPTION OF THE PRESSURE GAUGE A Bourdon tube pressure gauge is a mechanical instrument that uses a curved, flattened metal tube to measure fluid pressure. As pressure increases, the tube attempts to straighten out, and this movement is transferred through a linkage mechanism to a pointer that indicates the pressure on a dial. These gauges are widely used, operate without electricity. They are widely used in LH2 storage tank and other LH2 systems. They are now made of AISI 316L stainless steel wetted parts to resist hydrogen permeation and embrittlement. In addition, they features an additional safety characteristics aiming at minimising consequences of explosion: a safety case to protect people standing in front of the instruments.

Operational Condition
Consequences
Number of Injured Persons
0
Number of Fatalities
0
Environmental Damage
0
Property Loss (onsite)

low

Property Loss (offsite)

0

Post-event Summary

Damage probaly only the cost of the gauge

Event Nature
Emergency Action

Safety measures worked as planned: the alarm sounded, the system was isolated and then vented.

Release Type
Release Substance
H2 100%
Hydrogen Release Concentration (%)
0.00
Ignition Source
References
References

Mishap no 68 in P. L. Ordin, Review of hydrogen accidents and incidents in NASA operations, 1974, NASA TM X-71565 https://ntrs. nasa. gov/citations/19740020344

Lowesmith et al. , Safety issues of the liquefaction, storage and transportation of liquid hydrogen: An analysis of incidents and HAZIDS, Int. J. Hydrogen energy (2014) https://doi. org/10. 1016/j. ijhydene. 2014. 08. 002

Hankinson and Lowesmith, Qualitative Risk Assessment of Hydrogen Liquefaction, Storage and Transportation, FCH JU project IDEALHY, Deliverable 3. 10 (2013) confidential (accessed October 2025)