Release of hydrocarbons mixture from a pressure vessel
A release of contents of a pressure vessel occurred when a longitudinal weld tore open. The vessel had been shut down and had just been put into use again when the incident occurred. The gas mixture contained hydrocarbons with 30% hydrogen. It had reached its working pressure of 31 bar, but was only at -26 degrees C, instead of the working temperature of -73 degrees C, no liquid was present. An investigation found a crack, 1. 6 metres long, had formed near the upper end of the weld.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Causes

The recommendations issued after the incident, suggest that the ROOT CAUSE could be a lack of proper inspection, and/or inspection performed with inadequate tools