Failure of a pipe a ammonia plant due to hydrogen embrittlement
The incident happened in an ammonia plant, on the pipe leading hot synthesis gas (syngas) from the synthesis convertor to the first heat exchanger. The pipe cracked, releasing the syngas which did not produce “No serious fire occurred”. This pipe had already experienced six previous failures and consequent leakages. Following each cracking, repair/re-welding was performed. Before the last cracking, part of the pipe had been replaced with a new piece. All cracks occurred at the same location, an approximately 90 degrees bend of the pipe. The scientific article used as source (see references) reports that the design and the material adopted for the pipe was correct, and the pipe was operated within the recommended temperature and hydrogen partial pressure limits. Most of the cracks were due to hydrogen embrittlement and/or insufficient heat treatment in the welds and their heat affected zones. Additional causes were additional local microstructural aspects contributing to degrading the mechanical performance of the bend in respect to the design values assumed for the base material.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Cause Comments
The INITATING CAUSE was the cracking of a pipe and the consequent release of syngas. The referred scientific article reported the following findings: 1. All six failures could be attributed to incorrect heat treatment. 2. Their modified microstructure failed due to hydrogen embrittlement. 3. The geometric deformation in the bending caused a doubling of the stresses of the straight (and perfectly round) pipe The ROOT CAUSE could be then identified in inadequate design and component manufacturing.