Skip to main content

Bolts rupture due to hydrogen embrittlement (175)

This data is from the European Hydrogen Incidents and Accidents database HIAD 2.1, European Commission, Joint Research Centre.

Bolts rupture due to hydrogen embrittlement

The bolts on a not further specified industrial facility failed after approximately 4000 hours in service (approximately 18 months in service). Their failure bolts causedH2S leaks. The bolts fractured as a result of a hydrogen embrittlement mechanism (Hydrogen Stress Cracking) in a H2S rich atmosphere and in presence of humidity.
Event Date
December 1, 2003
Record Quality Indicator
Region / Country
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Cause Comments
The cause was a material/component failure due to hydrogen embrittlement (Sulphide Stress Cracking). The steel used for the bold belonged to a martensitic steel family which is not advised for use for continuous operation with wet H2S. The ROOT CAUSE could be attributed to a design failure.
Facility Information
Application Type
Application
Unknown
Specific Application Supply Chain Stage
Components Involved
Bolts
Storage/Process Medium
Storage/Process Quantity
0
Location Type
Operational Condition
Consequences
Number of Injured Persons
0
Number of Fatalities
0
Lessons Learned
The specific hydrogen-related damage causing the rupture of the bolts is known as Sulphide Stress Cracking (SSC). In first instance, the steels react with hydrogen sulphide (H2S), forming metal sulphides (MeS) and atomic hydrogen as corrosion byproducts. SSC is basically a hydrogen embrittlement phenomenon, in which atomic hydrogen penetrates in the steel cracking it. It is a mechanism susceptible to occur when 3 circumstances take place simultaneously: a susceptible material, a brittle atmosphere (H2S) and a sufficient maintained level of stresses. It is a mechanism that can happen under mechanical loads of remarkably lower magnitudes than the elastic limit of the material, being able to be sufficient the own residual stresses of manufacturing or assembly. Susceptibility to hydrogen embrittlement of steels is as much greater as it is its mechanical resistance or hardness, a reference value of 26 HRC being used for martensitic stainless steels with quenching and tempering thermal treatment (In this case, bolts had a hardness 48 HRC).
Event Nature
Release Type
Release Substance
H2S 100%
Hydrogen Release Concentration (%)
0.00
Ignition Source
Detonation
No
Deflagration
No
High Pressure Explosion
No
High Voltage Explosion
No
References
References

source lost