Release of a light hydrocarbon gas mixture in a chemical product plant
During the start-up operation (phase) of a cryogenic unit, a separator exploded, releasing ethane, ethylene, methane and hydrogen. The bursting of a tank was caused by a 1600 mm long incipient crack which had been formed at the inside of the tank along a weld line (a ferritic basis metal had been welded with an austenitic weld metal). The hydrogen induced incipient crack (cracking) was caused by the alternating load during start-up and shut-down phases in the course of the operating time.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Cause Comments
The INITIATING CAUSE was hydrogen induced cracking originated by the geometric form variation and the resulting plastic deformation in the area of a longitudinal seam weld. This incipient cracking was favoured by the high tensile (strength) austenitic CrNiMnW weld metal with its particularly accentuated martensitic composite (mixed) zone (area) along the transition between weld metal and basis metal and was also favoured by its physical characteristics which differ strongly from the basis metal. Possible ROOT CAUSES could two contributions: (i) a wrong execution of the welding (wrong choice of materials, inadequate themral management), aand a a lack of inspection / maintenance.