metal degradation in components of a refinery
This event regards the degradation of steels used in the heat-exchangers of a reformer of a refinery. An inspection by non-destructive ultrasonic techniques revealed material degradation of the steel components. The opening of the equipment confirmed the analysis: blisters were visible on metal sheets and cracks were present on welded parts. The material was an 0. 5% Molybdenum steel.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Causes
Cause Comments
The INITIATING CAUSE was degradation of gas pipes and other components due to high-temperature hydrogen attack This is a near miss. If the degradation of the steel components would have not been detected on time, the hydrogen attack would have proceeded until a loss of confinement, with release of hydrogen-reach process gas I the heat exchangers. Similar incidents have brought to extensive fire and damage to plants. The ROOT CAUSE would be an inadequate design, tens of years before, due to lack of scientific knowledge on the sensitivity of the specific steel used to hydrogen attack.