Hydrogen fire in a refinery
A hydrogen leak occurred on the hydrogen line of a hydro-desulphurisation unit, followed by ignition . The failure was located on a supply manifold of the unit at a support beam. The unit was shut down. The accident was caused by external corrosion which had developed at a support point, under the pipe insulation. A regular thinning of the piping was observed over a length of 450 mm on the lower semi-circumference. The maximum thickness loss was 6. 5 mm. The mechanical analysis concluded that the operating pressure was sufficient to cause this initial failure in the weakened area. Its propagation resulted from the dynamic load applied to the line.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Causes
Cause Comments
INITIATING CAUSE was the thinning of the pipe wall caused by external, not further specified corrosion. The ROOT CAUSE is not provided, but by proxy with similar cases, it could be concluded that lack of correct non-distructive assessment system did not allow for timely detection of the loss of wall thickness due to corrosion.