hydrogen fire in the hydro-desulphurisation unit of a refinery
A hot oil line (8-inch) in the hydro-desulphurisation (HDS) unit failed due to fatigue cracking. Hot oil at 50 bar and 343°C sprayed across the roadway into the hydrogen units where ignition occurred. The pipe break was a guillotine -type, probably in the heat affected zone at 2 inches from a welding. The intense fire around the pipe rack in the hydrogen plant caused a hydrogen line (16-inch) to rupture, adding a second blow torch to the fire. In successive order, more pipes ruptured with explosions. After six-and-a-half hours, the fire was extinguished. Damage was extensive. The three hydrogen units and the four HDS units were heavily damaged or destroyed.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Cause Comments
The INITIATING cause is fatigue cracking of the oil pipeline, different sources referring to probable fatigue cracking, again probably hydrogen assisted. Before the loss, the line which failed was judged as having excessive vibration. Failure of managing out-of-specification fatigue phenomena may be the root cause, or at least a contributing cause.