Fire of a mixture of hydrogen and hydrocarbons in a refinery
The fire occurred on the tube plate gaskets of 3 of the 4 exchangers loaded with catalytic reforming effluent. The fuel (500°C and p=30 bar) was a mixture of 30% hydrocarbons and 70% hydrogen. After depressurisation of the unit and nitrogen flushing (some problems to access the valves), the exchangers being cooled (overall flow 600 m³/h on 3 units), the fire was controlled until extinction by nitrogen injection. The accident was apparently due to incorrect tightening of the threaded rods; only 1/5 were correctly tightened on one of the heat exchangers involved. Three threaded rods break and the gasket surfaces were poorly prepared.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Causes
Cause Comments
The INITIATING cause was the release of hydrogen at a flange The root (or interm4ediate) cause was the wrong execution of the flange joint (incorrect tightening, bad quality of the gasket surface)