Explosion on the hydro-treatment unit of a refinery
The release and fire occurred during what appeared to be a normal operation in a reactor section of a Residue Hydrotreater Unit, when an eight-inch pipe connected to a heat exchanger failed at the flange. Recycled gas, primarily hydrogen, was suddenly released when the pipe broke away. The hydrogen, under high pressure and temperature, was ignited, sending a large jet fire shooting an estimated 75 feet westward from the flange. Damage was localized along that fire path. Initial information indicated the hydrogen was pressurized at approximately 3,000 psi (approximately 210 bar) ) at a temperature of over 500 F (260 C). Heat from the fire deformed piping and bent structural beams.
Event Initiating System
Classification of the Physical Effects
Nature of the Consequences
Cause Comments
The INITIATING cause was the failure of a carbon steel elbow, severely weakened by high temperature hydrogen attack and ruptured after operating for only 3 months. According to the CSB bulletin (see references), the investigation determined that the 8-inch diameter carbon steel elbow had been installed inadvertently in a high-pressure, high-temperature hydrogen line during a maintenance. The contractor accidentally switched a carbon steel elbow with an alloy steel elbow during a scheduled heat exchanger overhaul in February 2005. The alloy steel elbow was resistant to high temperature hydrogen attack (HTHA) but the carbon steel elbow was not. The maintenance contractor was unaware of the material differences in the elbows and the plant operator did not require the contractor to implement any special precautions to prevent inadvertently switching the elbows or any post-reassembly testing to confirm the alloy elbows were reinstalled in the correct locations. These findings suggest at a ROOT CAUSE related to organisation, specifically in maintenance control and contractor management.